About ASTM A387 Steel Plate
- Thickness: 5-100mm
- Length: 2000mm, 4000mm, or as required
- Width: 1000mm, 1500mm, or as required
- Application: steel boiler plate, pressure vessel plate
- Supplementary Technology: Annealing, normalizing plus tempering, or when the buyers agreed, Using blast or liquid quenching method accelerated cooling from austenitizing temperature, followed by tempering.
- Surface: Coated or Shot Blasting and Painting
- Delivery state: Hot Rolled, Cold Rolled
- Steel Grade: Grade 2, Grade 12, Grade 11, Gr.22, Gr.22L, Gr.21, Gr.21L, Gr.5, Gr.9, Gr.91
Product Scope:
ASTM A387 specification covers chromium-molybdenum alloy steel plates for welded boilers and pressure vessels manufactured for elevated temperature service. Available steel plate grades are 2, 12, 11, 22, 22L, 21, 21L, 5, 9 and 91. Steel product shall be killed and heat treated. The petrochemical, hydrocarbon processing and coal conversion industries have been utilizing this steel for decades, it varies according to the chromium and molybdenum. Most commonly used are Grade 12, 11, 22, and 5. Further more, these grades are available in 2 strength levels-class1 and class2.
ASTM A387 steel plate are typically applied in the temperature range from 316℃ to 593℃. The elevated temperature properties of these alloy steel plates are still of particular usage, now, ASTM A387 steel plate are manufactured to be fine grain, low silicon, low sulfur, calcium treated and occasionally produced Q&T to give the highest levels of toughness.
ASTM A387 Chemical Composition:
Chemical Requirements for ASTM A387 Pressure Vessel Plates | |||||||||||
---|---|---|---|---|---|---|---|---|---|---|---|
Elements | Gr.2 | Gr.12 | Gr.11 | Gr.22 | Gr.22L | Gr.21 | Gr.21L | Gr.5 | Gr.9 | Gr.91 | |
S50460 | K11757 | K11789 | K21590 | K21590 | K31545 | K31545 | S50200 | K90941 | K90901 | ||
Carbon, max | 0.04-0.21 | 0.04-0.17 | 0.04-0.17 | 0.04-0.15A | 0.12 max | 0.04-0.15A | 0.12 max | 0.15 max | 0.15 max | 0.06-0.15 | |
Manganese | 0.50-0.88 | 0.35-0.73 | 0.35-0.73 | 0.25-0.66 | 0.25-0.66 | 0.25-0.66 | 0.25-0.66 | 0.25-0.66 | 0.25-0.66 | 0.25-0.66 | |
Phosphorous, max | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | |
Sulfur, max | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.025 | 0.012 | |
Silicon | 0.13-0.45 | 0.13-0.45 | 0.44-0.86 | 0.50 max | 0.50 max | 0.50 max | 0.50 max | 0.55 max | 1.05 max | 0.18-0.56 | |
Chromium | 0.46-0.85 | 0.74-1.21 | 0.94-1.56 | 1.88-2.62 | 1.88-2.62 | 2.63-3.37 | 2.63-3.37 | 3.90-6.10 | 7.90-10.10 | 7.90-9.60 | |
Molybdenum | 0.40-0.65 | 0.40-0.65 | 0.40-0.70 | 0.85-1.15 | 0.85-1.15 | 0.85-1.15 | 0.85-1.15 | 0.40-0.70 | 0.85-1.15 | 0.80-1.10 | |
Nickel, max | - | - | - | - | - | - | - | - | - | 0.43 | |
Vanadium | - | - | - | - | - | - | - | - | 0.05 max | 0.16-0.27 | |
Columbium | - | - | - | - | - | - | - | - | - | 0.05-0.11 | |
Nitrogen | - | - | - | - | - | - | - | - | - | 0.025-0.080 | |
Aluminum, max | - | - | - | - | - | - | - | - | - | 0.02 | |
Titanium, max | - | - | - | - | - | - | - | - | - | 0.01 | |
Zirconium, max | - | - | - | - | - | - | - | - | - | 0.01 | |
1. The carbon content for plates over 5 in. [125 mm] in thickness is 0.17 max on product analysis2. Measured on round test specimens.3. Measured on flat specimen. |
ASTM A387 Mechanical Property:
Tensile Requirements for ASTM A387 Class 1 Pressure Vessel Plates | |||
---|---|---|---|
Grade 2 and 12 | Grade 11 | Grade 22, 21, 5, 9, 21L, 22L | |
Tensile Strength Ksi(Mpa) |
55~80 (380~550) |
60~85 (415~585) |
60~85 (415~585) |
Yield Strength, min Ksi(Mpa) |
33(230) | 35(240) | 30(205) |
Elongation in 8 in.[200mm], min, % | 18 | 19 | - |
Elongation in 2 in.[50mm], min, % | 22 | 22 | 18 |
Reduction of area, min, % | - | - |
45B 40C |
Tensile Requirements for ASTM A387 Class 2 Pressure Vessel Plates | |||||
---|---|---|---|---|---|
Grade 2 | Grade 11 | Grade 12 | Grade 22, 21, 5, 9 | Grade 91 | |
Tensile Strength Ksi(Mpa) |
70~90 (485~620) |
75~100 (515~690) |
65~85 (450~585) |
75~100 (515~690) |
85~110 (585~760) |
Yield Strength, min Ksi(Mpa) |
45(310) | 45(310) | 40(275) | 45(310) | 60(415) |
Elongation in 8 in.[200mm], min, % | 18 | 18 | 19 | - | - |
Elongation in 2 in.[50mm], min, % | 22 | 22 | 22 | 18 | 18 |
Reduction of area, min, % | - | - |
45B 40C |
- |
ASTM A387 Equivalent steel grade:
BS | EN | ASTM/ASME | DIN |
---|---|---|---|
621 B | ––– | SA387-11-2 | ––– |
622-515B | 10 CRMO910 | SA387-22-2 | 10 CRMO910 |
620 B | 13 CRMO 45 | SA387-12-2 | 13 CRMO 44 |
––– | ––– | SA387-9-2 | ––– |
––– | ––– | SA387-91-2 | ––– |
If you are interested in buying ASTM A387 steel plate products, contact us now for the latest price or check the following table for equivalent steel grade of ASTM A387.
We receive enquiries in English, Español (Spanish), Русский язык (Russian), Français (French) and العربية (Arabic). Our professional team will reply to you within one business day. Please feel free to contact us!